Matters needing attention when welding ductile iron pipes

May 06, 2022

1. Check the stress, deformation, level of difficulty in operation and the thickness of the weldment, welding position and diameter of the electrode to prepare the corresponding groove.

2. Use flame to grill both sides of the part to be welded, so that all the oil that penetrates into the outside of the base body is volatilized until there is no smoke.

3. When welding, the arc should be low, the arc should be pressed quickly to avoid the arc, and the arc should not jump left and right to make the weld shape narrow and reduce the thermal stress area, which will make the ductile iron pipe connection high.

4. Adopt short arc and short weld welding, and the length of individual weld shall not be 60mm; Adopt intermittent sectional welding, weld one section at a certain distance, and then weld the next section; The interlayer temperature of multi-layer welding shall be controlled at 60~80 ℃, and the weld of the next layer shall be on the fusion line of the weld of the previous layer as far as possible; Inspection shall be carried out in time during welding. In case of air holes, slag inclusions, weld beading, etc., the weld shall be cleaned by hand grinding wheel immediately before welding the next layer.

5. When the weld is red hot, tap the weld with a small hammer until the weld becomes dark, to roll out the weld, relax the stress and squeeze the stingy hole, and at the same time refine the grains in the weld area.