1. Fake ductile iron pipes are prone to folding. Folds are various fold lines formed on the surface of ductile iron pipes, and this defect often runs through the longitudinal direction of the entire product. The reason for the folds is that due to the pursuit of the fake and inferior manufacturers, the reduction amount is too large, resulting in ears, and folding occurs during the next rolling.
2. The appearance of fake and inferior ductile iron pipes often has a pockmarked surface. The pockmarked surface is a defect of irregular irregularities on the surface of the ductile iron pipe due to serious wear of the rolling groove. Due to the pursuit of profit by manufacturers of fake and inferior ductile iron pipes, the rolling groove rolling often exceeds the standard.
3. The surface of the fake and inferior ductile iron pipe is prone to scarring. There are two reasons:
1) The material of fake and inferior ductile iron pipes is uneven and there are many impurities.
2) The guide equipment of the fake and inferior material manufacturers is simple and easy to stick to the steel. These impurities are prone to scarring after biting the roll.
4. The surface of the fake and inferior material is prone to cracks, because its blank is adobe, and the adobe has many pores. During the cooling process, the adobe is subjected to thermal stress, resulting in cracks. After rolling, there are cracks.
5. The fake and inferior ductile iron pipes are easy to be scratched, because the fake and inferior materials manufacturers have simple equipment, which is easy to produce burrs and scratch the surface of the ductile iron pipes. Scratches reduce the strength of ductile iron pipes.
6. The fake and inferior ductile iron pipes have no metallic luster and are light red or similar to pig iron. There are two reasons:
1) Its blank is adobe.
2) The rolling temperature of fake and inferior materials is not standard, and their steel temperature is measured by visual inspection, so that it cannot be rolled according to the specified austenite area, and the performance of ductile iron pipes will naturally fail to meet the standard.
7. The transverse ribs of the fake and inferior ductile iron pipes are thin and low, and the phenomenon of full filling often occurs. The reason is that the manufacturer has to achieve a large negative tolerance, the reduction amount of the first few passes of the finished product is too large, the iron shape is too small, and the hole shape is not full.
8. The cross section of the fake and inferior ductile iron pipe is oval. The reason is that in order to save materials, the reduction amount of the first two passes of the finished roll is too large. standard.
9. The composition of the ductile iron pipe is uniform, the tonnage of the cold shearing machine is high, and the end face of the cutting head is smooth and tidy. However, due to the poor material of the fake and inferior material, the end face of the cutting head often has the phenomenon of meat loss, that is, unevenness and no metallic luster. And because the products of the fake and inferior material manufacturers have less cutting heads, there will be big ears at the head and tail.