Corrosion failure analysis of stainless steel pipe fittings

Apr 21, 2023

1. Stress corrosion: Stainless steel pipe fittings produce stress corrosion in the corrosive medium environment containing oxygen and chloride ions. The proportion of stress corrosion failure is as high as about 45%.

Common protective measures: Reasonable material selection and stress corrosion resistant materials mainly include high-purity austenitic chromium-nickel steel, high-silicon austenitic chromium-nickel steel, high-chromium ferritic steel and ferritic-austenitic dual-phase steel. Among them, ferrite-austenite dual-phase steel has the best stress corrosion resistance. Stress control: During assembly, try to reduce stress concentration, and make the part in contact with the medium have the minimum residual stress, prevent bumps and scratches, and strictly abide by the welding process specifications.

Strictly abide by the operating procedures: strictly control the process indicators such as raw material composition, flow rate, medium temperature, pressure, and pH value. Add corrosion inhibitor within the range allowed by the process conditions. When chromium-nickel stainless steel pipe fittings are used in dissolved oxygen chloride, the mass fraction of oxygen should be reduced to below 1. 0×10 - 6 . Practice has proved that in water containing 500. 0 × 10 - 6 mass fraction of chloride ions, it is only necessary to add a mixture of nitrate with a mass fraction of 150. 0 × 10 - 6 and sodium sulfite with a mass fraction of 0. 5 × 10 - 6 , You can get good results.

2. Pitting corrosion failure and preventive measures

Small hole corrosion is generally easy to occur in static media. Corrosion pits usually develop along the direction of gravity or transverse direction, and once the pitting corrosion is formed, it will automatically accelerate to the depth. , The oxide film on the surface of the stainless steel pipe fittings is dissolved in the aqueous solution containing chloride ions. As a result, small corrosion pits with a pore size of 20 μm to 30 μm are formed on the base metal. These small corrosion pits are pitting nuclei. As long as the medium contains a certain amount of chloride ions, the corrosion nuclei may develop into corrosion pits.